Henkel Loctite Ablestik 285 Thermally Conductive Adhesive Black 1 qt Can

Part number: PF285B
Henkel Loctite Ablestik 285 Thermally Conductive Adhesive Black 1 qt Can
Quantity Price
1 $132.05 132.050000000 USD New Limited Availability PF285B
2-9 $101.68 101.680000000 USD New Limited Availability PF285B
10+ $94.42 94.420000000 USD New Limited Availability PF285B
Item is currently on backorder and will be shipped as soon as possible.
  • A Made in the USA

Henkel Loctite Ablestik 285 Black, formerly Emerson and Cuming ECCOBOND, is a thixotropic, epoxy adhesive paste that is designed to be used with a catalyst for applications exposed to cryogenic temperatures as well as bonding ceramics, metal, and heat sinks. It offers a low coefficient of thermal expansion, non-sagging, versatility, low stress bonds, and excellent thermal cycling properties. 1 qt Can.

<p>Henkel Loctite Ablestik 285 Black, formerly Emerson and Cuming ECCOBOND, is a thixotropic, epoxy adhesive paste that is designed to be used with a catalyst for applications exposed to cryogenic temperatures as well as bonding ceramics, metal, and heat sinks. It offers a low coefficient of thermal expansion, non-sagging, versatility, low stress bonds, and excellent thermal cycling properties. 1 qt Can.</p>
Typical Use: Used for bonding metals and ceramic substrates in heat sink applications or any application that requires a thermally conductive adhesive.
Brand: Ablestik
Chemical Composition: Epoxy
Color: Black
Components: 2 part
Cure Time: Catalyst 9: 16 to 24h @ 25 °C; 11: 8 to 16h @ 80 °C; Catalyst 23LV: 16 to 24h @ 25 °C
Dielectric Strength: Catalyst 9: 17.7 kV/mm; Catalyst 11: 17.7 kV/mm; Catalyst 23LV: 17.7 kV/mm
Flash Point: >93.3 °C
Mix Ratio: Catalyst 9: 100:8.5 by volume, 100:3.5 by weight; Catalyst 11: 100:9.9 by volume, 100:4 by weight; Catalyst 23LV: 100:17 by volume, 100:7.3 by weight
Service Temperature: Catalyst 9: -40 to 130 °C; Catalyst 11: -55 to 155 °C; Catalyst 23LV: -65 to 105 °C
Shear Strength: Catalyst 11: 2,100 @ 25 °C
Specific Gravity: 2.4
Thermal Conductivity: Catalyst 9: 1.44 W/mK; Catalyst 11: 1.44 W/mK; Catalyst 23LV: 1.22 W/mK
Viscosity: Thixotropic paste
Volume Resistivity: Catalyst 9: 1 x 10^15 ohm-cm; Catalyst 11: 1 x 10^15 ohm-cm; Catalyst 23LV: 1 x 10^15 ohm-cm
Working Time: Catalyst 9: 45min; Catalyst 11: 4h; Catalyst 23LV: 60min

 